MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis Borcoat" HE7405 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Borcoat HE7405 is a polyethylene (PE) compound. The product is black colored and available in powder form for spray application.

Applications: Steel pipe coating Borcoat HE7405 is recommended to be used as an anti-slip "rough coat" layer on top of three-layer-PE based anti-corrosion coatings for steel pipes. Rough coat may be applied for/when: PE coated steel pipes are installed in steep terrain to increase friction with the surrounding ground; Increased safety during handling and loading operations; PE coated steel pipes on which a concrete weight coating is applied; Offshore pipes without concrete weight coating to improve the grip in the caterpillar clamps during laying operations

Specifications: Borcoat HE7405 and/or articles produced from it, are expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures. DNVGL-RP-F106; EN ISO 21809-1

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ISO 1183-1/Method A
Particle Size <= 150 µm<= 150 µm0-20%; ASTM D1921
 150 - 212 µm150 - 212 µm5-10%; ASTM D1921
 212 - 300 µm212 - 300 µm10-40%; ASTM D1921
 300 - 425 µm300 - 425 µm20-45%; ASTM D1921
 425 - 500 µm425 - 500 µm0-40%; ASTM D1921
 500 - 600 µm500 - 600 µm0-10%; ASTM D1921
Oxidative Induction Time (OIT) >= 20.0 min
@Temperature 210 °C
>= 20.0 min
@Temperature 410 °F
ISO 11357-6
Melt Flow 8.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.00 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Storage Temperature <= 50.0 °C<= 122 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FISO 11357-3
Vicat Softening Point >= 105 °C
@Load 1.02 kg
>= 221 °F
@Load 2.25 lb
A50; ISO 306
 
Descriptive Properties
Moisture Content<400 ppmKarl Fischer-titration, ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9623 / 322980

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.