MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Permatex® Black Silicone Adhesive Sealant
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Permatex® Black Silicone Adhesive Sealant (low odor formula) is a general purpose, single component, room temperature vulcanizing (RTV) compound, designed for the sealing of mechanical assemblies. Upon curing from the exposure to moisture in the air, this non-sagging paste forms a tough, flexible, waterproof seal of silicone rubber, which resists aging, weathering and thermal cycling without hardening, shrinking or cracking. Not recommended for engine gasketing applications or windshield installation.

Permatex® Black Silicone Adhesive Sealant cures on exposure to moisture in the air. The product dries tack free in 1 hour and fully cures in 24 hours. Cure times will vary with temperature, humidity and gap.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccUncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 18>= 18
Tensile Strength >= 1.17 MPa>= 170 psi
Elongation at Break >= 350 %>= 350 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
 260 °C500 °F
Minimum Service Temperature, Air -59.4 °C-75.0 °F
 -59.4 °C-75.0 °F
Flash Point >= 93.3 °C>= 200 °F
 
Processing PropertiesMetricEnglishComments
Extrusion Rate >= 250 g/min>= 250 g/minUncured
Cure Time 10100 min
@Temperature 25.0 °C
168 hour
@Temperature 77.0 °F
50% Relative Humidity. As Tested
 
Descriptive Properties
Chemical TypeOxime silicone rubber
ColorblackNon-sag paste. Uncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWP9161 / 239671

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.