Product Description: PA 66, Unfilled, Heat Stabilized, Lubricated, Black Color Availability: North America Additive: Heat Stabilizer; Impact Modifier; Lubricant Features: Heat Stabilized; Impact Modified; Lubricated RoSH Compliance: RoSH Compliant Appearance: Black Information provided by Ravago Manufacturing Americas |