MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Envalior Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Glass Fiber Reinforced

Material Notes: Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:
  • Highest mechanical properties at high temperatures
  • Excellent resistance to wear and low friction
  • Outstanding flow for easy processing and exceptional design freedom
  • Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties

Key Applications:

  • Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensioners
  • E&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliances

    Information provided by DSM.

    Former DSM Engineering Plastics product line is now with Envalior.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.68 g/cc0.0607 lb/in³(DAM); ISO 1183
    Water Absorption 5.9 %5.9 %DAM; Sim. to ISO 62
    Moisture Absorption at Equilibrium 1.6 %1.6 %Humidity Absorption (DAM); Sim. to ISO 62
    Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inDAM; ISO 294-4
     0.011 cm/cm0.011 in/inDAM; ISO 294-4
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength at Break 125 MPa18100 psiISO 527-1/-2
    Elongation at Break 3.5 %3.5 %ISO 527-1/-2
    Tensile Modulus 8.00 GPa1160 ksiISO 527-1/-2
    Charpy Impact Unnotched  5.00 J/cm²
    @Temperature -30.0 °C
    23.8 ft-lb/in²
    @Temperature -22.0 °F
    ISO 179/1eU
     6.00 J/cm²
    @Temperature 23.0 °C
    28.6 ft-lb/in²
    @Temperature 73.4 °F
    ISO 179/1eU
    Charpy Impact, Notched  0.900 J/cm²
    @Temperature -30.0 °C
    4.28 ft-lb/in²
    @Temperature -22.0 °F
    ISO 179/1eA
     1.10 J/cm²
    @Temperature 23.0 °C
    5.24 ft-lb/in²
    @Temperature 73.4 °F
    ISO 179/1eA
    Tensile Creep Modulus, 1000 hours 7500 MPa1.09e+6 psiISO 899-1
     
    Electrical PropertiesMetricEnglishComments
    Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
    Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
    Dielectric Constant  4.5
    @Frequency 1e+6 Hz
    4.5
    @Frequency 1e+6 Hz
    IEC 60250
     10
    @Frequency 100 Hz
    10
    @Frequency 100 Hz
    IEC 60250
    Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243-1
    Dissipation Factor  0.0070
    @Frequency 1e+6 Hz
    0.0070
    @Frequency 1e+6 Hz
    IEC 60250
     0.033
    @Frequency 100 Hz
    0.033
    @Frequency 100 Hz
    IEC 60250
    Comparative Tracking Index 250 V250 VIEC 60112
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 295 °C563 °F10°C/min (DAM); ISO 11357-1/-3
    UL RTI, Electrical  140 °C
    @Thickness 1.50 mm
    284 °F
    @Thickness 0.0591 in
    UL746B
     140 °C
    @Thickness 1.50 mm
    284 °F
    @Thickness 0.0591 in
    UL746B
    UL RTI, Mechanical with Impact  110 °C
    @Thickness 0.750 mm
    230 °F
    @Thickness 0.0295 in
    UL746B
     125 °C
    @Thickness 1.50 mm
    257 °F
    @Thickness 0.0591 in
    UL746B
    UL RTI, Mechanical without Impact  120 °C
    @Thickness 0.750 mm
    248 °F
    @Thickness 0.0295 in
    UL746B
     125 °C
    @Thickness 1.50 mm
    257 °F
    @Thickness 0.0591 in
    UL746B
     
    Descriptive Properties
    Flame RetardantYes
    Flame Retarding AgentYes
    Heat Stabilized or Stable to HeatYes
    Injection MoldingYes
    LubricantsYes
    PlatableYes
    Release AgentYes
    With FillersYes

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Akro-Plastic Akromid® T1 GF 50 (3101) PPA Conditioned, 50% Glass Filled
    Envalior Stanyl® TE250F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
    Shinkong Synthetic Fibers Shinite® D201 PBT
    Envalior Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
    BASF Ultrason® E 2010 PES

    PDSMEU464 / 31353

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.