MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 716K01 Radio Opaque Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 716K01 is a low viscosity epoxy resin system specifically developed for adhesive coating applications where radio opacity is required. This two part dark grey adhesive is commonly used for bonding, laminating and repair applications by manufactures of catheters, guide wires, stents, processing and packaging equipment, hearing aids, dental products and other biomedical instruments and devices. TRA-BOND 716K01 provides low permeability to gases and vapors and good resistance to water, weather, galvanic action, to petroleum solvents, lubricants, and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 13000 cP
@Temperature 25.0 °C
Mixed (cp #52, 10 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 911 hr @ 65°C
Adhesive Bond Strength 3500 psiLap shear, alum to alum, 1 hr @ 65°C
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 87.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 65.0 °C
 
Descriptive Properties
Color AmberHardener
 Dark GrayResin/Mixed/Cured
Thixotropic Index 1.31 rpm/10 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC139 / 71067

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.