MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sinotek Materials ZSKP100 Expandable Graphite
Categories: Carbon; Graphite

Material Notes: Expandable Graphite still retains the characteristics of natural flake graphite, and also has good expandability, loose and porous. Its heat-resistant range under the oxygen-free environment is between -200 to 3000°C, and it is chemically stable under high temperature, pressure or radiation. When the Expandable Graphite was treated in a twinkling at high temperature, the form of flake is turned into that of worm, and the volume can expand from 100 to 400 times. It is widely used in the dynamic and static seals in petroleum industry, chemical industry, electric industry, space industry, and automobile industry, etc.

Information provided by Sinotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 10 %<= 10 %
pH 3.0 - 7.03.0 - 7.0
Ash <= 8.0 %<= 8.0 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 90 - 99.9 %90 - 99.9 %
H2O, Water <= 1.0 %<= 1.0 %
Sulfur, S <= 0.10 %<= 0.10 %
 
Descriptive Properties
Expansion Ratio %100-200
Particle Size, Screen Oversize %, minimum80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating
BACT Dylyn® Diamond-Like Nanocomposite Coating
BACT DLC Diamond-Like Coating
Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95%

CSINOT39 / 2096

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.