MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott B270™ Sheet Glass
Categories: Ceramic; Glass; Optical

Material Notes: B 270™ crown glass in sheet glass form. Manufactured by the up-draw method, offers high stability with respect to solarization in combination with high transmission in the visible wavelength range. It has a fire-polished surface and high chemical stability. It is used in a variety of screens, monitors, touch panels, etc.

Information provided by SCHOTT North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.55 g/cc
Thickness <= 17000 micronswide range available
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 7.0
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.40 µm/m-°C
@Temperature 20.0 - 300 °C
Transformation Temperature, Tg 533 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5229
@Wavelength 588 nm
nd
Transmission, Visible 91.7 %
@Thickness 2.0 mm
TvD65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott N-BK7 Glass
Trinseo PULSE™ B-270 PC/ABS
Zeon Specialty Materials ZEONEX® 350R Cyclo Olefin Polymer
Schott N-PK51 Glass
301 Stainless Steel

CSGS129 / 138089

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.