MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. The key features of Styrodur C are high compressive strength, low water absorption, and outstanding thermal insulation. It is also rot-proof and easy to handle on site. Compressive strength is the major factor that differentiates the various grades of Styrodur C.

Applications: Domestic floors, Cavity walls, Conventional flat roofs, Parapet walls, Pitched roofs, Sandwich panels, and Warehouses

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0280 g/ccDIN EN 1602
Water Absorption 0.20 %by immersion; DIN EN 12087
 <= 3.0 %by diffusion; DIN EN 12088
Water Vapor Transmission 100 - 200 g/m²/dayDIN EN 12086
Deformation <= 5.0 %
@Pressure 0.0400 MPa,
Temperature 70.0 °C
DIN EN 1605
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 0.150 MPa
Creep Strength 0.0600 MPa
@Strain <=2 %
Compressive; long-term; 50 years; DIN EN 1606
 0.0800 MPa
@Strain <=2 %
Compressive; DIN EN 1606
 0.100 MPa
@Strain <=2 %,
Time 3.60e+6 sec
Compressive; mid-term; DIN EN 1606
Modulus of Elasticity 0.0150 GPaDIN EN 826
Tensile Modulus 15.0 MPa
Flexural Strength 0.500 MPa
Compressive Strength 0.150 - 0.200 MPa
@Strain 10 %
DIN EN 826
Compressive Modulus 10.0 MPaElasticity; Short term E; DIN EN 826
Shear Strength 0.200 MPa
 0.300 MPaAllowable
Adhesive Bond Strength <= 0.100 MPaon concrete
 <= 0.100 MPaon mineralic surfaces
 <= 0.100 MPaon gluing mortar
 <= 0.100 MPaon plasters
 >= 0.200 MPaon metals
 >= 0.200 MPaon wood
 >= 0.200 MPaon plastic
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°CDIN 53752
CTE, linear, Transverse to Flow 60.0 µm/m-°CDIN 53752
Thermal Conductivity 0.0330 W/m-KMoisture Content: 0%
 0.0340 W/m-KMoisture Content: 1%
 0.0340 W/m-KMoisture Content: 2%
 0.0350 W/m-KMoisture Content: 3%
 0.0350 W/m-KMoisture Content: 4%
 0.0360 W/m-KMoisture Content: 5%
 0.0370 W/m-KMoisture Content: 6%
 0.0380 W/m-KMoisture Content: 8%
 0.0390 W/m-KMoisture Content: 10%
 0.0400 W/m-KMoisture Content: 12%
 0.0240 W/m-K
@Temperature -80.0 °C
 0.0260 W/m-K
@Temperature -60.0 °C
 0.0280 W/m-K
@Temperature -40.0 °C
 0.0300 W/m-K
@Temperature -20.0 °C
 0.0320 W/m-K
@Temperature 0.000 °C
 0.0330 W/m-K
@Temperature 10.0 °C
 0.0340 W/m-K
@Temperature 20.0 °C
 0.0350 W/m-K
@Temperature 30.0 °C
 0.0360 W/m-K
@Temperature 40.0 °C
 0.0370 W/m-K
@Temperature 50.0 °C
 0.0300 W/m-K
@Thickness 20.0 mm
DIN EN 13164
 0.0310 W/m-K
@Thickness 30.0 mm
DIN EN 13164
 0.0320 W/m-K
@Thickness 40.0 mm
DIN EN 13164
 0.0330 W/m-K
@Thickness 50.0 mm
DIN EN 13164
 0.0340 W/m-K
@Thickness 60.0 mm
DIN EN 13164
Maximum Service Temperature, Air 75.0 °CDIN EN 14706
 
Descriptive Properties
Commercial StatusEurope
Dimensional Stability at Heat< 5%70°C, 90% rh; DIN EN 1604
Dynamic Stiffness120-800 MN/m3
Freeze-Thaw-Resistance<1%DIN EN1209

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe)

PBASG0086 / 131720

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.