MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Phillips 66 XD ISO Grade 460 Bearing Oil
Categories: Fluid; Lubricant

Material Notes: XD Bearing Oil is a high-performance antiwear circulating oil specifically developed for use in Morgan Construction No-Twist® rod mills. It provides excellent wear protection and rapid water separation for use in rod and bar mill rolling applications. XD Bearing Oil is formulated to provide good oxidation resistance, excellent wear protection, protection against rust and corrosion, and resistance to foaming. It has good oxidation resistance and thermal stability at high temperatures to minimize sludge and varnish formation, and provide long service life. It has excellent antiwear properties to help protect the gears, shafts, bearings and adjusting screws during the extrusion process. It has excellent water-separating properties to minimize the formation of emulsions in circulating systems subject to contamination with large quantities of water. It protects system components against rust and corrosion, and is resistant to excessive foam buildup that can interfere with proper lubrication.

Applications:

  • Morgan, Danieli, Demag and Pomini rod and bar mills
  • Circulating oil for ferrous and non-ferrous rolling mills
  • Circulating systems where water contamination is a problem
  • Large, slow-speed gears in mixers and mills
  • Hot and cold strip mills
XD Bearing Oil meets the requirements of the following OEM specification:
  • Morgan MMC40003 (ISO VG 100)
Features/Benefits:
  • Excellent wear protection
  • Excellent water-separating properties
  • Good oxidation resistance and thermal stability
  • Protects against rust and corrosion
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.894 g/cc
Density 7.45 lb/gal
Viscosity Measurement 95Index
Saybolt Viscosity at 100°F 2478 SUS
Saybolt Viscosity at 210°F 149 SUS
Kinematic Viscosity at 40°C (104°F) 462 cSt
Kinematic Viscosity at 100°C (212°F) 30.4 cSt
Oxidative Stability 3.73 hourRPVOT; ASTM D2272
ASTM Color 5.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.65[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.330 mmScar Diameter; ASMT D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -12.0 °C
Flash Point 270 °CCOC
 
Descriptive Properties
Copper Corrosion1bASTM D130
Demulsibility0 mlEmulsion @ 82°C, ASTM D2711
 0.004Water in Oil @ 82°C, ASTM D2711
 25 minutes to passASTM D1401
 36 mlFree water @ 82°C, ASTM D2711
FZG Scuffing Test12 Failure Load StageASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON6379 / 210088

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.