MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis ME1254 MDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: ME1254 is a fully formulated, medium-density polyethylene compound, containing an Azodicarbonamide (ADCA)-free chemical blowing agent, for chemically foamed telesingles.

Typical characteristics:

  • Outstanding extrusion stability
  • Consistent cell structure
  • Good surface finish
  • ADCA-free
Applications:
  • Dry core and petroleum jelly filled cables
  • Foam or foam-skin insulation for telephone singles and data cable with typical expansion of 35-40%.
Specifications: ME1254 is expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures. EN 50290-2-23; EN 60811-408

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.600 g/cc
Density 0.943 g/ccISO 1183-1
Oxidative Induction Time (OIT) >= 60.0 min
@Temperature 600 °C
ISO 11357-6
Melt Flow 0.950 g/10 min
@Load 5.00 kg,
Temperature 140 °C
ISO 1133-1
Storage Temperature 10.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 58.0
@Time 1.00 sec
ISO 868
Tensile Strength 11.0 MPa25 mm/min; ISO 527-2
 11.0 MPa25 mm/min, expanded ( 38 %) insulation; IEC 60811-408
Elongation at Break 500 %25 mm/min; ISO 527-2
 500 %25 mm/min, expanded ( 38 %) insulation; IEC 60811-408
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.32
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.000500
@Frequency 1e+6 Hz
ASTM D150
 
Processing PropertiesOriginal ValueComments
Processing Temperature 100 °CConductor preheating
Zone 1 110 °C
Zone 2 145 °C
Zone 3 190 °C
Zone 4 205 °C
Zone 5 220 °C
Die Temperature 220 °C
Melt Temperature 220 °C
Shelf Life 18.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9815 / 323172

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.