MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
High-leaded brass, 62%, UNS C35300
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Combines excellent machinability with moderate cold workability.

Applications: gears, wheels, nuts, plates for clocks, keys, bearing cages, engraver's plates, pinions, valve stems.

Available as flat products and rod.

Key Words: free-cutting brass, FC brass, CDA 353, CZ131, ISO CuZn37Pb2, CEN CW606N
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 338 - 586 MPa
Tensile Strength, Yield 117 - 427 MPaDepending on temper
Elongation at Break 52 %in 127 mm.
Modulus of Elasticity 105 GPa
Poissons Ratio 0.346
Machinability 90 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 39.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.3 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
Melting Point 885 - 910 °C
Solidus 885 °C
Liquidus 910 °C
Annealing Point >= 800 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 600 °C
Hot-Working Temperature 785 - 815 °C
Recrystallization Temperature 320 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 62 %
Lead, Pb 1.8 %
Zinc, Zn 36.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nickel Aluminum Bronze, UNS C63000, Annealed Rod
Free-Cutting Brass, UNS C36000
Forging Brass, UNS C37700
High-leaded brass, UNS C34200
Cartridge Brass, UNS C26000 (260 Brass), OS100 Temper flat products

MC35300b1 / 11232

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.