MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TROGAMID® CX9710 Polyamide
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Properties: Common transparent polyamides consist in partially aromatic units that impart rigidity and high heat resistance. Our TROGAMID® T5000 is a typical representative of this group. Replacing aromatic constituents with aliphatic monomers improves the UV stability of transparent polyamides. TROGAMID® CX7323 is an example of this type of polyamides. By selecting specific monomers, one can achieve a crystallizable and permanently transparent polyamide: TROGAMID® CX. The crystallites are so small that they do not scatter visible light, and the material appears transparent to the human eye—a property known as microcrystallinity. Because of its crystallinity, the microcrystalline structure retains important properties such as stress cracking resistance— without clouding. The degree of crystallinity is so negligible, however, that it has no adverse effect on the shrinkage behavior of molded parts. TROGAMID® CX undergoes a similar isotropic shrinkage like amorphous materials. TROGAMID® CX combines the chemical resistance of semi-crystalline molding materials with the advantages of amorphous, UV-resistant materials. The outstanding properties of TROGAMID® CX are:
  • crystal-clear, permanent transparency, high transmission
  • superior chemical and stress cracking resistance
  • high level of UV resistance
  • low water absorption compared with many other polyamides, which leaves the mechanical properties virtually unaffected
  • very balanced mechanical property profile
  • high dimensional stability
  • high impact resistance, even at low temperatures
  • high level of dynamic strength (e.g., for internally pressurized parts)
  • abrasion and scratch resistance
  • high glass transition temperature
  • very low isotropic shrinkage
  • easy processing
The combination of good UV resistance, high mechanical strength, permanent transparency, high transmission and superior chemical resistance opens a wide range of applications for TROGAMID® CX. Typical areas of application are in the auto motive industry, machinery and engineering, medical technology, the sports and recreation industry, the glasses production, the cosmetics industry and in water treatment and filter technology.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Viscosity Number >= 150 cm³/g
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81ISO 868
Ball Indentation Hardness 110 MPaH30; ISO 2039-1
Tensile Strength, Yield 48.0 MPa
@Temperature 80.0 °C
50 mm/min; ISO 527-1/2
 60.0 MPa
@Temperature 23.0 °C
50 mm/min; ISO 527-1/2
Elongation at Break >= 50 %
@Temperature 80.0 °C
50 mm/min; ISO 527-1/2
 >= 50 %
@Temperature 23.0 °C
50 mm/min; ISO 527-1/2
Elongation at Yield 5.5 %
@Temperature 80.0 °C
50 mm/min; ISO 527-1/2
 8.0 %
@Temperature 23.0 °C
50 mm/min; ISO 527-1/2
Tensile Modulus 1270 MPa
@Temperature 80.0 °C
ISO 527-1/-2
 1400 MPa
@Temperature 23.0 °C
ISO 527-1/-2
Flexural Strength 9.00 MPa5 mm/min, outer fiber strain at max stress; ISO 178
 50.0 MPa5 mm/min, 3.5% at strain; ISO 178
 90.0 MPa5 mm/min; ISO 178
Flexural Modulus 1.70 GPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature 0.000 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 14.0 kJ/m²
@Temperature 0.000 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 1400 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 700 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
IEC 60250
 3.6
@Frequency 100 Hz
IEC 60250
Dielectric Strength 27.0 kV/mmIEC 60243-1
Dissipation Factor 0.0115
@Frequency 100 Hz
IEC 60250
 0.0325
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 575 V100 drops value; IEC 60112
 600 VCTI; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 122 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 108 °CISO 75-1/-2
Vicat Softening Point 130 °C
@Load 5.10 kg
ISO 306
 135 °C
@Load 1.02 kg
ISO 306
Glass Transition Temp, Tg 140 °CISO 11357
Flammability, UL94 HB
@Thickness 0.800 mm
IEC 60695
 HB
@Thickness 1.60 mm
IEC 60695
Glow Wire Ignition Temperature 775 °C
@Thickness 1.00 mm
IEC 60695
Glow Wire Flammability Index 800 °C
@Thickness 1.00 mm
IEC 60695
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TROGAMID® CX9704 Polyamide
Evonik Trogamid® T-GF35 35% Glass Reinforced Amorphous Nylon
Domo TECHNYL® A 216 PA66, Conditioned
Evonik Trogamid® BX9723 30% Glass Fiber Reinforced Polyamide
Evonik Trogamid® CX7337 nf Transparent Nylon

PEVONIL199 / 196403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.