MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
3M Jet-melt™ 3797 Lt. Grey Adhesive: High-Melt Technology  (discontinued **)
Categories: Polymer; Adhesive; Thermoset

Material Notes: The flash point is 570°F (299°C). The auto ignition is 700°F (371°C). The ball and ring soft point is 304°F (151°C); ASTM E-28-6-7. The peal strength on canvas is 10 PIW at 72°F (22°C). The bonding range of a 1/8 inch bead on Douglas Fir to Douglas Fir is 30 seconds. The delivery rate is 55 seconds for 1 inch x 3 inch cartridge. The ingredients of the product when dried after application are listed as indirect food additives under FDA regulation 21 CFR 175.105.

Good electrical properties, good flow and heat resistance for potting.

Information provided by 3M Adhesives Division.

Key Words: 3M Adhesives Division
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 2650 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1.95 MPa
Elongation at Break 98 %
Adhesive Bond Strength 2.41 MPa
@Temperature 22.2 °C
on Douglas Fir
Impact Test 1.02 J
@Temperature -17.8 °C
 19.0 in-lb
@Temperature 22.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 77.0 °CHeat Resistance Temp
Flammability, UL94 V-2
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMMA16 / 53363

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.