MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt SILVALOY® 560 (Braze™ 560, Silvaloy® A56T FC) Silver-Copper-Zinc Alloy Flux Coated Rod (AWS BAg-7)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvaloy 560 Flux Coated Rod consists of a 0.062" diameter filler rod that is coated with a precise coating of flux to a final diameter of 0.125". Silvaloy 560 is a silver based brazing alloy used for ferrous and non-ferrous alloys in joints requiring a low temperature, cadmium-free alloy, as in food handling equipment.

Information provided by Lucas-Milhaupt.

Key Words: AMS 4763
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 9.42 g/cc9.42 g/cc
Density 9.41 g/cc0.340 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000208 ohm-cm0.0000208 ohm-cm8.32% IACS
 
Thermal PropertiesMetricEnglishComments
Melting Point 618.3 - 651.7 °C1145 - 1205 °F
Solidus 618.3 °C1145 °F
Liquidus 651.7 °C1205 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 651.7 - 760 °C1205 - 1400 °FBrazing Range
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 21 - 23 %21 - 23 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 55 - 57 %55 - 57 %
Tin, Sn 4.5 - 5.5 %4.5 - 5.5 %
Zinc, Zn 15 - 19 %15 - 19 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NLUCM9891 / 254808

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.