MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Inhance Fluoro-Seal INHANCE® KF Aramid Fiber Pulp
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Aramid

Material Notes: Product Description: INHANCE KF fiber is an aramid fiber pulp that has been surface activated by a proprietary reactive gas process. Surface activation makes the fibers easy to disperse, and creates superior adhesion between the fiber and the surrounding polymer.

Applications: Add INHANCE KF fibers to coatings, adhesives and sealants as a stable thixotrope for excellent viscosity control. Also INHANCE KF fibers added to urethanes, epoxies, polyesters (BMC, SMC) and other polymers create reinforced composites that capture the unique benefits of aramid while also experiencing enhanced dispersion and adhesion. Benefits include increased tensile strength, increased tear resistance, and superior abrasion resistance.

Fiber Characteristics: 12 micron diameter

Fiber Length (avg.): 0.03 in.

Information provided by Inhance/Fluoro-Seal, Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.44 g/cc
Bulk Density 0.0800 g/cc
Surface Tension 55 dynes/cmwater wettable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell Spectra® S--900 650-926 Fiber
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Mitsui Fybrel® E 380 Polyolefin Synthetic Pulp, Dry Processes
Milliken® MilliCap® 9919 Aramid
Lanxess Rhenogran® AFP-40/EPDM (GE 1909) Aramid Fiber Pulp

PINHAN009 / 137220

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.