MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Smooth-Cast® 385 Mineral Filled Urethane Casting Resin
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: Smooth-Cast™ 385 is a mineral filled urethane casting resin that is very hard and durable. When Parts A and B are mixed in proper proportion (1A:5B by weight), Smooth-Cast™ 385 cures at room temperature with virtually no shrinkage. This rigid urethane casting resin has high compressive and flexural strength. Fully cured castings are tough, machinable and paintable. Color effects are possible by adding pigment dispersions. They resist moisture and mild solvents. Smooth-Cast™ 385 is ideal for making industrial production parts, foundry patterns, vacuum forming molds, and some ceramic applications.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D-1475
Viscosity 3000 cP3000 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.00060 cm/cm0.00060 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D-2240
Tensile Strength, Ultimate 21.4 MPa3100 psiASTM D-638
Elongation at Break 1.0 %1.0 %ASTM D-638
Tensile Modulus 2.76 GPa400 ksiASTM D-638
Flexural Strength 40.7 MPa5900 psiASTM D-790
Flexural Modulus 2.99 GPa433 ksiASTM D-790
Compressive Strength 58.6 MPa8500 psiASTM D-695
Compressive Modulus 2.76 GPa400 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 57.0 °C135 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min2.00 hourHandling Time
Pot Life 20.0 min20.0 minASTM D-2471
 
Descriptive Properties
ColorBeige
Mix Ratio1A:1Bby weight
Specific Volume17.3[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN028 / 296729

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.