MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

Compliant with EC food contact regulations.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0330 g/cc0.00119 lb/in³Nominal skin/skin; BS ISO 7214 1998
 0.0280 - 0.0400 g/cc0.00101 - 0.00145 lb/in³sheet density
Cell Length 0.150 - 0.500 mm0.00591 - 0.0197 in
 0.350 mm0.0138 inTypical Diameter
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 555510 mm cell/cell thickness; ISO 868 1985
Tensile Strength 0.875 MPa127 psiISO 7214 1998
Elongation at Break 190 %190 %
Compressive Yield Strength  0.0520 MPa
@Strain 10 %
7.54 psi
@Strain 10 %
BS ISO 7214 1998
 0.0700 MPa
@Strain 25 %
10.2 psi
@Strain 25 %
BS ISO 7214 1998
 0.102 MPa
@Strain 40 %
14.8 psi
@Strain 40 %
BS ISO 7214 1998
 0.136 MPa
@Strain 50 %
19.7 psi
@Strain 50 %
BS ISO 7214 1998
Tear Strength 1.00 kN/m5.71 pliBS EN ISO 8067 1995
Compression Set  3.0 %
@Time 79200 sec,
Strain 25 %
3.0 %
@Time 22.0 hour,
Strain 25 %
24 hr recovery; BS ISO 7214 1998
 7.5 %
@Time 79200 sec,
Strain 25 %
7.5 %
@Time 22.0 hour,
Strain 25 %
0.5 hr recovery; BS ISO 7214 1998
 11 %
@Time 79200 sec,
Strain 50 %
11 %
@Time 22.0 hour,
Strain 50 %
24 hr recovery; BS ISO 7214 1998
 22.5 %
@Time 79200 sec,
Strain 50 %
22.5 %
@Time 22.0 hour,
Strain 50 %
0.5 hr recovery; BS ISO 7214 1998
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0390 W/m-K0.271 BTU-in/hr-ft²-°Fmean temp of 10°C; ISO 8302 1991
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Flammability Test  1.2
@Thickness 13.0 mm
1.2
@Thickness 0.512 in
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 1.7
@Thickness 5.00 mm
1.7
@Thickness 0.197 in
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 
Descriptive Properties
FlammabilityAutomotive: FMVSS.302 burn ratePass: 6mm and thicker

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZOTEF939 / 150695

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.