MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Meyors Chemical Antioxidant SP/P
Categories: Other Engineering Material

Material Notes: Product Code: MSHQD-AN045-03 PT
Chemical Name: Mixture of Styrenated phennols and Silica
Trade Name: Antioxidant SP/P
CAS No.: 61788-44-1
Molecular Formula: C8n+6H9n+4O

Typical Properties: Montclair SP/P is a medium activity mon staining. Non-discoloring antioxidant for satex and solid runner formulations, and is a stabilizer for synthetic elastomers. Montaclere SP/P is a general-purpose antioxidant processing oxidation resistance and moderate heat aging resistance properties in NR, and in SBR, NBR, IR, BR and CR.

Recommended Applications: Because of this excellent color stability, it is widely used in white and light colored applications such as shoe soles general mechanical goods, carpet backing, flooring, sporting goods, and latex. Montaclere SP/P may reduce surface ”crazing” caused by UV light degradation. Montaclere SP/P may use alone or in combination with other antioxidants for the stabilization of synthetic elastomers. Montaclere SP/P is regulated for use in article in articles in contact with food as specified under FDA 21 CFR177.2600 ,175.105 and NgVV XXI, Caregoru 4, Santocures.

Information provided by Meyors Chemical INC Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 5.5 - 8.5
Viscosity 8000 cP
Ash 29 - 31 %
 
Descriptive Properties
AppearanceLight or off-white powder
Content60-65%Content of SP
Loss on drying<5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMEYORS015 / 316597

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.