MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sika Sikaflex® -2c NS Two-component, non-sag, polyurethane elastomeric sealant
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Sikaflex-2c NS is a 2-component, premium-grade, polyurethane-based, elastomeric sealant. It is principally a chemical cure in a non-sag consistency. Meets ASTM C-920, Type M, Grade NS, Class 25, use T, NT, M, G, A, O, I and Federal Specification TT-S-00227E, Type II, Class A. Tested in accordance with ASTM C-1382 for use in EIFS systems.

Where to use:

  • Intended for use in all properly designed working joints with a minimum depth of 1/4 inch.
  • Ideal for vertical and horizontal applications.
  • Placeable at temperatures as low as 40°F.
  • Adheres to most substrates commonly found in construction.
  • An effective sealant for use in Exterior Insulation Finish Systems (EIFS).
  • Submerged environments, such as canal and reservoir joints.
Advantages:
  • Capable of ±50% joint movement.
  • Chemical cure allows the sealant to be placed in joints exceeding 1/2 in. in depth.
  • High elasticity with a tough, durable, flexible consistency.
  • Exceptional cut and tear resistance.
  • Exceptional adhesion to most substrates without priming.
  • Available in 35 architectural colors.
  • Color uniformity assured via Color-pak system.
  • Available in pre-pigmented Limestone Gray (no Color-pak needed).
  • Non-sag even in wide joints.
  • Easy to mix.
  • Paintable with water-, oil-, and rubber-base paints.
  • Jet fuel resistant.

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 20 - 3020 - 30ASTM D2240
Tensile Strength 0.655 MPa95.0 psiASTM D412
Tensile Stress at Strain 0.483 MPa
@Strain 100 %
70.0 psi
@Strain 100 %
ASTM D412
Elongation at Break 500 %500 %ASTM D412
Tear Strength 7.89 kN/m45.0 pliASTM D624
Peel Strength 4.38 kN/m25.0 pliConcrete, 0% Adhesion loss; Fed Spec. TT-S-00227E
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 76.7 °C170 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 4320 min72.0 hourFinal cure; ASTM C-679
Tack-Free Time 360 - 480 min6.00 - 8.00 hourASTM C-679
Shelf Life 12.0 Month
@Temperature 4.00 - 35.0 °C
12.0 Month
@Temperature 39.2 - 95.0 °F
in original unopened cartridge
 
Descriptive Properties
ColorWide range availableSpecial colors on request

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIKA938 / 209845

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.