MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

NOVA Chemicals DYLITE® F271TNL Expanded Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Applications: Drinking cups (hot and cold), Take-out containers, Ice cream containers, Labeled and printed cups, Thin-wall cups at high density, Noodle bowls, Soup containers.

Attributes: Good thermal insulation, Superior temperature retention, Less exterior condensation, Strong and lightweight, Superior taste and odor properties, Superior barrier resistance to spicy, oils and foods, Improved leak resistance for hot and cold beverages.

Primarily engineered for higher densities >60 g/l or 3.75 pcf, Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliant, Pre-lubricated – no blending: Additional lubricant may be required depending on final part application.

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.609 - 0.641 g/cc0.0220 - 0.0231 lb/in³
Volatiles 5.3 - 5.9 %5.3 - 5.9 %Pentane, by weight
Bead Size 0.305 - 0.508 mm0.0120 - 0.0200 infine
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C35.0 µin/in-°F
Thermal Conductivity 0.0339 W/m-K0.235 BTU-in/hr-ft²-°FK-factor, Lambda
Insulation R Value 4.24.2per inch
Maximum Service Temperature, Air 79.4 °C175 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOV620 / 249077

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.