Description: This product is an industrial nonionic polydimethylsiloxane emulsion. Key Features - Industry leading particle size
- Excellent Freeze-thaw stability
- Great gloss and water repellency
- Easily dispersed with water with minimal agitation
Key Applications- Tire dressing
- Leather conditioning
- Rubber treatment
- Fiberglass treatment
Application: ICM 1670E is a 60% active emulsion of 350cst polydimethylsiloxane. Because of its non-ionic nature, it can be used in a variety of systems, such as nonionic, anionic, cationic surfactant or polymer systems without forming a complex.Addition Rates Dosage – 1: 1-5% Information provided by CHT Group |