MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teijin Tenax® E HTS40 F13 24K 1600tex Poly-acrylonitrile Carbon Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: HTS40 is a family of high strength/standard modulus aerospace grade carbon fibers made in Japan (E13- sized products) and Germany (F13-sized product) for use as reinforcement in high performance composites. These fibers are produced from poly-acrylonitrile (PAN) precursor and are surface treated to promote adhesion to organic matrix polymers. Sizing materials are designed to aid in handling. The -J HTS40 E13 3K/6K and the -E HTS40 F13 12K fibers have been qualified to the NMS 818 dry fiber specification. This allows manufacturers to call out an industry standard, PCD-controlled, aerospace-grade carbon fiber without the expense of writing and maintaining their own in-house specifications.

Information provided by Teijin Carbon America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 g/cc
Filament Diameter 7.0 µm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4400 MPa
Elongation at Break 1.9 %SACMA SRM16
Tensile Modulus 230 GPaSACMA SRM16
 
Descriptive Properties
Density1616 texLinear density without sizing
Sizing level (%)1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

ETEIJIN909 / 277919

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.