Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefin base containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution, toxic and corrosive gases and dark smoke emission. This material complies with RoHS requirements. Standard Complying - EN 50363-5 EI8; EN 50363-6 EM8 and EM10; EN 50264 EI101...EI104, EI106...EI109 and EM101...EM104; IEC 60092/360 HF90; IEC 60092 SHF2; Cenelec HD 624.6; VDE 0266 HXI1 and HXM1; VDE 0250 HI3; VDE 0207 HJ1, HM1 and HM3; BS 7655 LRS1 and SW3. Crosslinkable; Flame Retardant; Fuel Resistant; Halogen Free; Low Smoke Emission; Low Toxicity; Oil Resistant; Self Extinguishing Uses: Cable Jacketing; Low Voltage Insulation; Wire & Cable Applications Availability: Asia Pacific; Europe; North America Information provided by Solvay Specialty Polymers. |