MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Mobility and Materials Liveo™ BioMedical Grade LSR 7-6840
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Liquid Silicone Rubber raw materials for medical device and component fabrication in the Healthcare Industry

Information provided by DuPont. This was previously a Dow Corning product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.023 cm/cm0.023 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4242ASTM D 2240
Elongation at Break >= 300 %>= 300 %ASTM D 412
200% Modulus 2.40 MPa348 psiASTM D 412
Tear Strength 37.0 kN/m211 plidie B; ASTM D 624
Compression Set 44.2 %
@Temperature 23.0 °C
44.2 %
@Temperature 73.4 °F
ISO 815
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °FDuPont proprietary test
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Temperature 150 °C
0.0833 hour
@Temperature 302 °F
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
Polymer(Si)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4748 / 256197

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.