MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Micropol Microlin LL17 Linear Polyethylene Rotational Molding Powder
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: Information provided by Micropol Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D792
Melt Flow 4.0 - 6.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 10.0 MPa50mm/min; ASTM D638-64T
Elongation at Break 840 %ASTM D638-64T
Flexural Modulus 0.245 GPaASTM D760-66
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 91.0 °CASTM D1525
Brittleness Temperature <= -70.0 °CASTM D746
Flammability, UL94 V-2
Oxygen Index 26 %Critical
 
Descriptive Properties
British Standard 2782:508AZero Burn Rate
British Standard 476 Part 7Class 2
Civil Aviation Authority Spec No 8 Vertical TestPass
Stores Materials Container Fire TestPass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovation Polymers Nima™ HL 18400 HDPE
Avient Maxxam® FR PE JR 165 High Density Polyethylene (HDPE)
Avient Maxxam™ FR PE126 BLK 3330 Polyethylene, Low Density (LDPE)
Avient Maxxam™ FR PE 112 LDPE
Avient Maxxam® FR PE 125 Low Density Polyethylene, Wire and Cable

PMICRO00 / 53057

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.