MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Baybond® XL 825 Fluid
Categories: Fluid

Material Notes: Waterbased aliphatic blocked polyisocyanate. Baybond® XL 825 is suitable for use as a crosslinker for glassfiber sizings. In combination with Bayhydrol® polyols Baybond® XL 825 can be used for the formulation of water-reducible, lightfast one-component polyurethane baking coatings and as an additive in waterborne baking systems to improve flexibility, impact strength and adhesion.

Properties / Applications: Baybond® XL 825 was developed as crosslinker for the sizing of glass fibers used in combination with Baybond binders to reinforce thermoplastics, particularly polyamide. Glass fiber sizes based on Baybond® XL 825 are characterized by their good colorfastness, even at elevated temperatures. The mechanical film properties of sizings based on Baybond® XL 825 are developed fully by postcrosslinking at temperatures from 170 °C for a duration of 20 minutes. The product is compatible with the additives normally used in the formulation of glass sizes, e.g. adhesion promoters, lubricants, antistatic agents and plasticizers.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 69 - 71 %0.9-1.1g / 1h / 125°C, convection oven
pH 7.0 - 8.0
 
Descriptive Properties
Content10%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Baybond® PU 401 A Polyester Urethane Polymer
Covestro Baybond® XL 7270 Fluid
Covestro Baybond® VP LS 2277 Polyester Urethane Polymer
Covestro Baybond® PU 407 Polyester Urethane Polymer
Covestro Baybond® PU 406 Polyurethane

PCOVEST0076 / 201859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.