MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zircar Ceramics AL-CEM Alumina Cement
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Type AL-CEM Alumina Cement is a high purity alumina bonding agent used for bonding ZIRCAR® fibrous ceramic products to themselves, and as a coating cement to improve the hardness and oxidation resistance of substrates.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.95 g/cc0.0704 lb/in³
Solids Content 70 %70 %
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 1870 °C>= 3400 °F
Maximum Service Temperature, Air 1650 °C3000 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99.2 %99.2 %
SiO2 0.80 %0.80 %
 
Descriptive Properties
ColorWhite
Coverage7 ft21 Pint as 0.01" Layer on Fibrous Ceramic Insulation
Weight per Pint2 lbs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Ceramics AS-CEM Alumina-Silica Cement
Unifrax Fiberfrax® Topcoat™ 3000 Coating Cement
Unifrax Fiberfrax® QF-180™ Blue Coating Cement
Thermal Ceramics Kaocrete 249 C Low Cement Castables
Röhm Acrifix® 117 Acrylic Cement

CZIR009 / 2817

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.