MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radici RADILON® NeXTreme RV500HHR 3800 BK Nylon, 50% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: High Temperature polyamide injection molding grade, 50% glass fiber reinforced. Superior thermal resistance in contact with hot air. Black color. Suitable for demanding mechanical applications in very severe temperature conditions, where the parts must endure long term contact with hot air until 220-230 °C. Very good properties retention after ageing. Typical applications in automotive are under bonnet components, like turbo air ducts, intercooler end caps. This material can be processed with water conditioned tools.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: Heat stabilized or stable to heat

Industries: Automotive, Consumer Industry Goods

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ISO 1183
Moisture Absorption 1.20 %
@Thickness 2.00 mm
1.20 %
@Thickness 0.0787 in
50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 233 MPa33800 psi5mm/min; ISO 527-2/1A
Elongation at Break 2.7 %2.7 %5mm/min; ISO 527-2/1A
Tensile Modulus 17.85 GPa2589 ksi1mm/min; ISO 527-2/1A
Flexural Strength 358 MPa51900 psi2mm/min; ISO 178
Flexural Modulus 15.2 GPa2200 ksi2mm/min; ISO 178
Charpy Impact Unnotched  10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 11.0 J/cm²
@Temperature -30.0 °C
52.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.80 J/cm²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohm500V; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 295 °C563 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FISO 75/2Bf
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Flame Spread 0.000 mm/min
@Thickness 3.00 mm
0.000 in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
 
Processing PropertiesMetricEnglishComments
Melt Temperature 305 - 315 °C581 - 599 °F
Mold Temperature 90.0 - 100 °C194 - 212 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI117 / 313618

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.