MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AISI 6120 Steel (UNS G61200)
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Key Words: UNS G61200
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 862 MPa
Tensile Strength, Yield 648 MPa
@Strain 0.2 %
Elongation at Break 21 %
Modulus of Elasticity 201 - 209 GPa
Bulk Modulus 160 - 170 GPa
Poissons Ratio 0.27 - 0.30
Shear Modulus 81.0 - 82.0 GPa

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 6145 Steel (UNS G61450)
AISI 51B60H Steel, annealed 815°C (1500°F)
AISI 51B60H Steel, normalized 855°C (1570°F)
AISI 6118 Steel
AISI 6118H Steel

M6120 / 100236

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.