MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Silikony Polskie Polsil OM 1000 Methyl Silicone Fluid
Categories: Fluid; Lubricant; Silicone Base

Material Notes: The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gives the silicone fluids special usage properties. A surface covered with methyl silicone fluids reflects anti-adhesive properties, while the thin layer of oil remaining on it, is resistant to high temperature. Fluids may be sprayed both in the form of several-percent solution and non-diluted. In rubber processing also water emulsion of silicone fluids are used (Polsil® E), which are easy to dilute and apply.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1000 cP
@Temperature 25.0 °C
Storage Temperature <= 40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silikony Polskie Polsil OM 300 Methyl Silicone Fluid
Shin-Etsu Silicones KF-6004 Fluid
Shin-Etsu Silicones 562P Fluid
Shin-Etsu Silicones 541 Fluid
Nye Lubricants 435 (SO) Synthetic Oil

PPOLSI039 / 84339

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.