MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lyanchemicals Tech EXT-700 CPVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: CPVC is a thermoplastic produced by chlorination of polyvinyl chloride (PVC) resin, which is significantly more flexible and can withstand higher temperature than PVC. It is a high heat and corrosion resistantmaterial, and it has become an important engineering thermoplastic due to its relatively low cost, high heat distortion temperature, chemical resistance, outstanding mechanical, and dielectric, flame andsmoke resistance properties. CPVC was first commercialized by Noveon in the early 1960s and has since proven its value in a variety of industrial applications in which a high use temperature and excellentresistance to chemical are desirable. Uses include hot and cold water delivery pipes and industrial liquid handling. Besides pipe and fittings, many other industrial fluid-handling product are available in CPVCincluding pumps, valves , strainers, tower packing, and duct, as well as sheet for fabrication into tanks, duct, and tank lining.

Characteristics: Best flowabilty

Application: It is mainly used for injection molding

Information provided by Lyanchemicals Tech Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.700 g/cc
Volatiles <= 0.30 %GB/T2914
Particle Mesh Size >= 30 Mesh>99% Sieving; GB/T2916
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPaASTM D638
Izod Impact, Notched (ISO) 10.0 kJ/m²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point >= 105 °C
@Load 5.00 kg
ASTM D1525
Decomposition Temperature >= 120 °CThermal; GH-002
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 64 - 66 %GB/T7139
 
Descriptive Properties
AppearanceWhite Power

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLYANT007 / 318034

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.