MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

MarkeTech BGO (Bismuth Germanate, Bi4Ge3O12) Scintillator Crystal  (discontinued **)
Categories: Ceramic; Oxide

Material Notes: Bismuth germanate is intrinsic scintillation material with high absorption power. Due to its high effective atomic number and high density, BGO is a very efficient gamma absorber with high photo effect fraction which results in a very good photo peak to Compton ratio. BGO detectors are preferred for medium and high-energy gamma counting and high-energy physics applications.

Data provided by MarkeTech International. MarkeTech International is no longer in business.

Key Words: Bi4Ge3O12, Bismuth Germanium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.13 g/cc0.258 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 5.05.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 µm/m-°C3.89 µin/in-°F
Melting Point 1050 °C1920 °F
 
Descriptive Properties
Crystal StructureCubic
Hydroscopic?No
Luminescence: Afterglow<0.005%at 6 ms
Luminescence: Decay Constant300 n/s
Luminescence: Integrated Light Output15-20NaI:Tl = 100
Luminescence: Photon Yield2 to 3300K; 103 pH/MeV
Luminescence: Radiation Length1.1 cm
Luminescence: Wavelength of max emissions480 nm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corning Pyrex® 7740 Borosilicate Glass Sheet
AISI 4130 Steel, annealed at 865°C (1585°F), furnace cooled 11°C (20°F)/hour to 680°C (1255°F), air cooled, 25 mm (1 in.) round
Corning 0211 Zinc Borosilicate Glass
Germanium, Ge
Corning 7761 Potash Borosilicate Crushed/Powdered Glass

C5MT836 / 120745

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.