MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® DD-10682 Silicone Microwave Absorber
Categories: Polymer; Thermoset; Silicone

Material Notes: Description:
  • Flexible, loaded, silicone, rubber microwave absorber.
  • Provides excellent attenuation across a wide frequency range.
  • The high magnetic loss of DD-10671 works well in suppressing resonant cavity modes, isolating signals, and attenuating surface currents.
  • Custom sheet sizes available upon request.
  • Available with pressure sensitive adhesive(PSA).
  • Can be water-jet or die cut for custom configurations.
  • Halogen free, RoHS and REACH compliant./ul>

    Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 40.0 milStandard
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87.0ASTM D2240
Tensile Strength 0.750 ksiASTM D638
Elongation at Break 75.0 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.10e+10 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 190 °C
Flammability, UL94 V-0
 
Descriptive Properties
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9448 / 322604

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.