MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This product complies with ASTM standard D1248-IA4 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: High clarity films coextruded with Polyamides, PVdC, EVOH, etc., for food packaging: cheese, ham, meat, sausages, etc. Cast films. Small flexible bottles.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Petroquimica Triunfo has been acquired by Braskem.

Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 - 0.924 g/cc0.0333 - 0.0334 lb/in³ASTM D1505
Thickness 50.0 microns1.97 mil
Melt Index of Compound 0.80 - 1.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 13.5 MPa1960 psiASTM D638
Tensile Strength, Yield 12.0 MPa1740 psiASTM D638
Film Elongation at Break, MD 375 %375 %ASTM D882
Film Elongation at Break, TD 720 %720 %ASTM D882
Elongation at Break 490 %490 %ASTM D638
Secant Modulus, MD 0.116 GPa16.8 ksi5%; ASTM D882
Secant Modulus, TD 0.122 GPa17.7 ksi5%; ASTM D882
Coefficient of Friction, Dynamic 0.600.60ASTM D1894
Elmendorf Tear Strength, MD 7.80 g/micron198 g/milASTM D1922
Elmendorf Tear Strength, TD 7.20 g/micron183 g/milASTM D1922
Dart Drop Test 150 g0.331 lb(method A); ASTM D1709
Film Tensile Strength at Break, MD 23.0 MPa3340 psiASTM D882
Film Tensile Strength at Break, TD 21.0 MPa3050 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 98.0 °C208 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 7.5 %7.5 %ASTM D1003
Gloss 62 %62 %45° - Gardner; ASTM D2457
 100 %100 %@ 60° Gardner; ASTM D2457
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Processing Temperature 155 - 165 °C311 - 329 °FPlasticizing Zone
 165 - 175 °C329 - 347 °FMixture Zone
Feed Temperature 150 - 160 °C302 - 320 °F
Adapter Temperature 175 - 185 °C347 - 365 °F
Blow-up Ratio (BUR) 3.03.0Recommended
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wanshijie APET Sheet
Eastman 9921P PET Film
DuPont Teijin Films Mylar® WRL63 Polyester Film, 200 Gauge
DuPont Teijin Films Mylar® OB01 Polyester Packaging Film, 100 Gauge

PDAX098 / 29523

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.