MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Silpak SP-200-4 Flexible Polyurethane Foam, 4 lb/ft3
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SP-200-4 Flexible Polyurethane Foam is a two-component, self-skinning, non-CFC, polyurethane flexible foam system. This product offers excellent flow and fast de-molding times for increased production cycles. Thickness of skin can easily be controlled by proper mold temperature settings and the amount of mixed product packed in the mold. These foams can be hand mixed or machine dispensed. Small batch mixes are easily achieved using fast, aggressive mixing methods with larger mixes better achieved using a high shear mixing blade (Jiffy Mixer).

Features:

  • Self-skinning
  • Excellent Flow
  • Non-CFC
  • Fast de-molding times
Applications: Recommended for making molded components where low-density flexible foam is required such as armrests, head restraints, dashboards, crash pads, side panels, steering wheels, special effects, and puppets in the following industries:
  • Aircraft
  • Recreational Vehicle
  • Theater
  • Automobile
  • Furniture

Information provided by Silpak a division of Polytek Development Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccPart B
 1.17 g/ccPart A
Density 4.00 lb/gal
Viscosity 600 cPInitial, Part A
 1740 cPInitial, Part B
Storage Temperature 64.0 - 86.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 - 25.0 minDemold Time
 60.0 secCream Time
 90.0 - 120 secRise Time
Shelf Life 6.00 Month
 
Descriptive Properties
Colorwhite
Expansion Rate (volume)<14 times
Mix Ratio34% A : 66% Bby weight
 47 A : 100 Bby volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSILPAK011 / 318648

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.