MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Synfoam® SG-30 Syntactic Foam
Categories: Polymer; Thermoset

Material Notes: Castable. SynFoam SG is a unique, cost effective castable syntactic foam that provides low density and moderate strength. It is suitable for numerous marine and aerospace applications where machining of parts is either impractical or too expensive. SynFoam SG is also ideal for field repair due to its room temperature cure which also eliminates CTE problems that will arise with elevated temperature cures. SynFoam SG exhibits low shrinkage and is resistant to water, oils, and fuels. The castable nature of the syntactic eliminates the cost and waste associated with machining. SynFoam SG is available as 1, 2, and 5 gallon kits. Each kit contains an A and B side that must be mixed together prior to casting. Cure is achieved within 24 hours and full properties will be realized after 7 days at room temperature. Densities can be customized to the user's specifications. Please consult the appropriate instructions for limitations of depth of cure.

Information provided by Synfoam®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.449 - 0.513 g/cc0.0162 - 0.0185 lb/in³
Moisture Absorption <= 3.00 %<= 3.00 %24 hours @ depth
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 24.1 MPa3500 psi
Compressive Modulus 0.827 GPa120 ksi
Hydrostatic Design Basis 31.7 MPa4600 psi
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 95.0 °C203 °F
 
Descriptive Properties
Depth Rating (m)1500
Service Pressure (psi)1360

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSYNF041 / 192916

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.