Description: Unreinforced polyamide 66, medium viscosity, for injection molding. Available in: Asia Pacific and Latin America Product Applications: TECHNYL ® A 216 offers all of the primary properties of unreinforced polyamide 66, such as: thermal and mechanical properties , impact resistance, abrasion and chemical resistance. This product is used in a wide variety of industries, including: industrial tools , frame of fuel filter for automobile, household appliances (housings fasteners, cable ties, bottle caps). This product is available in a large range of colors, and special colors on request. DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe. |