MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Parker Chomerics CHO-BOND® 1035 Electrically Conductive Sealant
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Electrically conductive, one component RTV silicone which provides both environmental sealing and EMI/RFI shielding. This sealant, filled with silver-plated glass particles, contains no acetic acid, and cures in the presence of moisture.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 2.00 g/cc1.80 - 2.00 g/cc
Volatile Organic Compounds (VOC) Content 151 g/l151 g/l
Thickness 178 microns7.00 milRecommended
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 0.689 MPa>= 100 psiLap
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.050 ohm-cm<= 0.050 ohm-cmDC
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min
@Temperature 23.0 °C
168 hour
@Temperature 73.4 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
BinderSilicone
ConsistencyThin paste
Coverage21.3 cm2 / g
FillerAg/glass
Mix Ratio1-part
Working Life0.5 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics Tecknit SC-Consil® 860 Carbon-Filled Silicone Elastomer
Momentive Performance Materials Silopren™ LSR 2345/06 Electrically-Conductive Liquid Silicone Rubber
BIW ASTM Class 2D2 Silicone Foam

PCHOME021 / 28243

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.