MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Overview of materials for Zinc Alloy
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Zinc Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by alloying elements or processing methods.

Applications: corrosion protection (galvanization), architectural, automotive, batteries, toys.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 5.02 - 7.17 g/ccAverage value: 6.61 g/cc Grade Count:65
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 42.0 - 119Average value: 72.1 Grade Count:48
Hardness, Knoop 80.0 - 149Average value: 104 Grade Count:34
Hardness, Rockwell A 36.0 - 46.5Average value: 39.6 Grade Count:14
Hardness, Rockwell B 49.0 - 74.0Average value: 56.2 Grade Count:20
Hardness, Vickers 30.0 - 135Average value: 87.3 Grade Count:38
Tensile Strength, Ultimate 37.0 - 441 MPaAverage value: 259 MPa Grade Count:58
Tensile Strength, Yield 125 - 386 MPaAverage value: 277 MPa Grade Count:20
Elongation at Break 1.00 - 65.0 %Average value: 25.9 % Grade Count:54
Modulus of Elasticity 63.5 - 97.0 GPaAverage value: 83.2 GPa Grade Count:14
Compressive Yield Strength 210 - 641 MPaAverage value: 359 MPa Grade Count:12
Fatigue Strength 28.0 - 172 MPaAverage value: 60.1 MPa Grade Count:28
Fracture Toughness 12.3 - 23.7 MPa-m½Average value: 16.3 MPa-m½ Grade Count:6
Shear Strength 138 - 325 MPaAverage value: 225 MPa Grade Count:18
Charpy Impact, Unnotched 1.40 - 65.0 JAverage value: 34.5 J Grade Count:17
Coefficient of Friction 0.0300 - 0.0700Average value: 0.0500 Grade Count:4
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000580 - 0.00000840 ohm-cmAverage value: 0.00000621 ohm-cm Grade Count:56
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.4 - 39.9 µm/m-°CAverage value: 26.8 µm/m-°C Grade Count:56
Specific Heat Capacity 0.390 - 0.525 J/g-°CAverage value: 0.416 J/g-°C Grade Count:49
Thermal Conductivity 105 - 125 W/m-KAverage value: 109 W/m-K Grade Count:50
Melting Point 375 - 800 °CAverage value: 424 °C Grade Count:60
Solidus 375 - 441 °CAverage value: 404 °C Grade Count:54
Liquidus 382 - 502 °CAverage value: 424 °C Grade Count:54
 
Processing PropertiesOriginal ValueComments
Processing Temperature 393 - 538 °CAverage value: 456 °C Grade Count:3
Annealing Temperature 105 - 250 °CAverage value: 197 °C Grade Count:14
Hot-Working Temperature 120 - 300 °CAverage value: 225 °C Grade Count:37
Casting Temperature 395 - 545 °CAverage value: 460 °C Grade Count:16
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.00100 - 50.0 %Average value: 7.48 % Grade Count:70
Cadmium, Cd 0.00200 - 0.450 %Average value: 0.0252 % Grade Count:63
Copper, Cu 0.00100 - 6.00 %Average value: 1.01 % Grade Count:62
Iron, Fe 0.00200 - 0.100 %Average value: 0.0429 % Grade Count:63
Lead, Pb 0.00200 - 1.40 %Average value: 0.0658 % Grade Count:63
Magnesium, Mg 0.00500 - 0.100 %Average value: 0.0236 % Grade Count:31
Tin, Sn 0.00100 - 0.00500 %Average value: 0.00178 % Grade Count:61
Titanium, Ti 0.120 - 0.500 %Average value: 0.294 % Grade Count:7
Zinc, Zn 50.0 - 100 %Average value: 91.7 % Grade Count:73

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zinc, Zn
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Sand Cast
Overview of materials for Solder/Braze Alloy
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Permanent Mold Cast

M01075 / 81680

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.