MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik Alkrothal 720 Resistance Strip
Categories: Metal; Ferrous Metal; Ferritic; Superalloy; Iron Base

Material Notes: ALKROTHAL 720 is a ferritic FeCrAl alloy which is recommended for use at temperatures up to 1000°C (1830°F). Typical applications for ALKROTHAL 720 are in rheostats, braking resistors, etc. It is also used as electrical heating elements in industrial applications.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 200
Tensile Strength, Ultimate 550 MPa
 30.0 MPa
@Temperature 900 °C
deformation rate= 6.2x10-2/min
Tensile Strength, Yield 420 MPa
@Strain 0.2 %
Elongation at Break 20 %
Creep Strength 1.00 MPa
@Temperature 1000 °C,
Time 3.60e+6 sec
1% elongation
 4.00 MPa
@Temperature 800 °C,
Time 3.60e+6 sec
1% elongation
Modulus of Elasticity 220 GPa
 130 GPa
@Temperature 1000 °C
 150 GPa
@Temperature 800 °C
 170 GPa
@Temperature 600 °C
 190 GPa
@Temperature 400 °C
 205 GPa
@Temperature 200 °C
 210 GPa
@Temperature 100 °C
Poissons Ratio 0.30
Shear Modulus 85.0 GPacalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000120 ohm-cm
 0.000120 ohm-cm
@Temperature 100 °C
 0.000122 ohm-cm
@Temperature 200 °C
 0.000123 ohm-cm
@Temperature 300 °C
 0.000123 ohm-cm
@Temperature 400 °C
 0.000126 ohm-cm
@Temperature 500 °C
 0.000129 ohm-cm
@Temperature 600 °C
 0.000130 ohm-cm
@Temperature 700 °C
 0.000132 ohm-cm
@Temperature 800 °C
 0.000133 ohm-cm
@Temperature 900 °C
 0.000133 ohm-cm
@Temperature 1000 °C
 0.000134 ohm-cm
@Temperature 1100 °C
Curie Temperature 600 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 - 250 °C
 12.0 µm/m-°C
@Temperature 20.0 - 500 °C
 14.0 µm/m-°C
@Temperature 20.0 - 750 °C
 15.0 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
 0.630 J/g-°C
@Temperature 200 °C
 0.720 J/g-°C
@Temperature 400 °C
 0.730 J/g-°C
@Temperature 1000 °C
 0.800 J/g-°C
@Temperature 800 °C
 1.00 J/g-°C
@Temperature 600 °C
Thermal Conductivity 16.0 W/m-K
@Temperature 20.0 °C
Melting Point 1500 °C
Maximum Service Temperature, Air 1000 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.70fully oxidized
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 4.0 %
Carbon, C <= 0.080 %
Chromium, Cr 12 - 14 %
Iron, Fe >= 80.52 %
Manganese, Mn <= 0.70 %
Silicon, Si <= 0.70 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Alkrothal 14 Resistance Strip
Sandvik Alkrothal 3 Resistance Strip
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled
Carpenter Invar 36® Alloy, Cold Rolled Strip

NSANDV062 / 18956

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.