MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) RHODOLINE® WA 265 Surfactant
Categories: Fluid

Material Notes: Standard Applications: RHODOLINE® WA 265 N is an APE free wetting and dispersing agent for paints and pigments dispersions. The optimum dosage should be checked in each case individually. Typically, 0.1-0.6% would be used in coatings formulations, whereas 2-15% would be required as a vehicle for a pigment concentrate.

Chemical Name: Wetting and Dispersing Agents

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³
pH 5.0 - 7.05.0 - 7.0in water; RPG02
 
Thermal PropertiesMetricEnglishComments
Pour Point <= 5.00 °C<= 41.0 °F
Flash Point >= 100 °C>= 212 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 5.0<= 5.0RPG18
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.3 Month24.3 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 9.0 - 11 %9.0 - 11 %RPG16
 
Descriptive Properties
AppearanceClear to slightly hazy liquid
Content11.8HLB Number
 90%Active
Ionic ChargeNonionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAFAC® RE-610 E Surfactant
Rogers Arlon T4015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Rogers Arlon T3030-R004 0.030" (0.762 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Rogers Arlon T3020-R004 0.020" (0.508 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Rogers Arlon T3015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate

PSOLVAY811 / 218539

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.