MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Vinyl Dry Blend E7755 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8484ASTM D2240
Tensile Strength, Yield 43.4 MPa6290 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.92 GPa424 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 79.4 MPa11500 psiASTM D790
Flexural Modulus 3.01 GPa437 ksiASTM D790
Izod Impact, Notched 13.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
24.4 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
Dart Drop Total Energy  71.2 J/cm
@Temperature 23.0 °C
0.133 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 133 J/cm
@Temperature 23.0 °C
0.249 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.70e+15 ohm-cm
@Thickness 1.22 mm
7.70e+15 ohm-cm
@Thickness 0.0480 in
ASTM D257
Surface Resistance 4.70e+14 ohm
@Thickness 1.22 mm
4.70e+14 ohm
@Thickness 0.0480 in
ASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 61.0 µm/m-°C33.9 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 74.8 °C167 °Fconditioned @ 50 deg.C; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
@Thickness 3.18 mm
163 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94  HB
@Thickness 0.370 mm
HB
@Thickness 0.0146 in
white; UL 94
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
All Color; UL 94
 5VA
@Thickness 2.00 mm
5VA
@Thickness 0.0787 in
white; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 210 °C379 - 410 °F
 
Descriptive Properties
FeaturesGood Thermal Stability
 High Impact Resistance
FormsPowder
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Outdoor Suitabilityf1UL 746C
Processing MethodExtrusion
 Profile Extrusion
 Sheet Extrusion
PVC Cell Classification1-42434-33-0100ASTM D4216
 16354ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesFencing & Decking
 Film
 Outdoor Applications
 Profiles
 Sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® HN-1064IA PC, Unreinforced FR
Westlake Plastics Radel® R 5500 Polyphenylsulfone
Karina E 822-10/148-CRB-LMP White PVC Compound
Henkel Loctite® Shadowcure™ 5293 Silicone Coating
Geon® Performance Solutions M2150 Molding PVC; Opaque Grade

PH0POL0240 / 144809

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.