MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Endex™ 155 Hydrocarbon Resin
Categories: Polymer

Material Notes: Product Description: A water-white thermoplastic resin made from purified aromatic hydrocarbon monomers. Used to modify the melt flow and increase the temperature resistance of styrenic plastic and rubber. Reinforces the styrene end blocks of styrenic block copolymers. In adhesives Endex™ 155 hydrocarbon resin will associate with the styrenic endblocks, producing higher cohesion at temperatures up to 70°C without affecting tack and adhesion properties.

Application/Uses:

  • Assembly
  • Automotive
  • Building and Construction
  • Caulks and Sealants
  • Hot Melt Adhesives
  • Nonwovens
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Tapes and Labels
Key Attributes:
  • Heat stability
  • Pure aromatic monomer composition
  • Very high softening point
  • Water-white initial color

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
Viscosity 1000 cP
@Temperature 235 °C
Melt
 10000 cP
@Temperature 200 °C
Melt
 100000 cP
@Temperature 175 °C
Melt
Molecular Weight 2500 g/molMz
 6900 g/molMw. Mw/Mn ratio = 2.8
 12900 g/molMn
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 105 °C
Ring & Ball Softening Point 153 °CASTM E 28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0ASTM D6166
 
Descriptive Properties
Cloud Point117°COMS
 15°CMMAP
 -20°CDACP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5318 / 222512

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.