Pomalux® POMC CN-P (Statically conductive polyoxymethylene copolymer) is a conductive acetal copolymer. It is a carbon powder filled material that offers consistent surface resistivity in the 10ee4 to 10ee6 range. Properties of note include dimensional stability, strength, stiffness, and chemical resistance.. Colors Available: Black Attributes: Dielectric Properties; Chemical Resistance; Wear Resistance Shapes: Compression Sheet Information provided by Westlake Plastics Co. |