INNOPOL® CS 3-9230 KAR BU is a black colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer. INNOPOL® CS 3-9230 KAR BU is developed for producing injection molded components for household appliances. All information provided by INNO-COMP. |