MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® PC PC0703R PC (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC0703R resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market. It is available exclusively at www.sabicpc.com

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Water Absorption 0.35 %0.35 %23°C/sat; ISO 62
Moisture Absorption at Equilibrium 0.35 %0.35 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
6.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
cm³/10 min; ISO 1133
 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
 120120ISO 2039-2
Tensile Strength, Yield 63.0 MPa9140 psi50 mm/min; ASTM D638
 63.0 MPa9140 psi50 mm/min; ISO 527
Elongation at Break >= 70 %>= 70 %50mm/min; ISO 527
 >= 70 %>= 70 %50mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527
 6.0 %6.0 %50 mm/min; ASTM D638
Tensile Modulus 2.35 GPa341 ksi1mm/min; ISO 527
 2.35 GPa341 ksi50 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa13100 psi2 mm/min; ISO 178
 90.0 MPa13100 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.30 GPa334 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.30 GPa334 ksi2 mm/min; ISO 178
Izod Impact, Notched 9.00 J/cm16.9 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D4812
Izod Impact, Notched (ISO) 70.0 kJ/m²33.3 ft-lb/in²80*10*3; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
Dart Drop, Total Energy 65.0 J47.9 ft-lbpeak; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
 >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D257
Dielectric Constant  3.0
@Frequency 60 Hz
3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 60 Hz
3.0
@Frequency 60 Hz
IEC 60250
Dielectric Strength  27.0 kV/mm
@Thickness 1.60 mm
686 kV/in
@Thickness 0.0630 in
ASTM D149
 27.0 kV/mm
@Thickness 1.60 mm
686 kV/in
@Thickness 0.0630 in
IEC 60243-1
Dissipation Factor  0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
IEC 60250
 0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
ASTM D150
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
 70.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
38.9 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
 0.200 W/m-K1.39 BTU-in/hr-ft²-°FASTM C177
Hot Ball Pressure Test 125 °C257 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °C280 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 138 °C
@Thickness 3.20 mm
280 °F
@Thickness 0.126 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C261 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 127 °C
@Thickness 3.20 mm
261 °F
@Thickness 0.126 in
ASTM D648
Vicat Softening Point 144 °C291 °FRate B/50; ISO 306
 144 °C291 °FRate B/50; ASTM D1525
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
UL 94
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ISO 489
 1.5861.586ASTM D542
Haze <= 0.80 %
@Thickness 2.54 mm
<= 0.80 %
@Thickness 0.100 in
ASTM D1003
Transmission, Visible 88 - 90 %
@Thickness 2.54 mm
88 - 90 %
@Thickness 0.100 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 60.0 °C104 - 140 °FHopper Temperature
 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 280 - 310 °C536 - 590 °FInjection Molding
Zone 1 260 - 280 °C500 - 536 °FProfile Extrusion
 270 - 300 °C518 - 572 °F
Zone 2 260 - 280 °C500 - 536 °FProfile Extrusion
 280 - 310 °C536 - 590 °F
Zone 3 260 - 280 °C500 - 536 °FProfile Extrusion
 290 - 320 °C554 - 608 °F
Zone 4 260 - 280 °C500 - 536 °FProfile Extrusion
Adapter Temperature 260 - 280 °C500 - 536 °FProfile Extrusion
Die Temperature 250 - 260 °C482 - 500 °FProfile Extrusion
Melt Temperature 270 - 280 °C518 - 536 °F
 290 - 320 °C554 - 608 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 120 °C248 °FProfile Extrusion
 120 °C248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 2.00 - 4.00 hour2.00 - 4.00 hourProfile Extrusion
Moisture Content 0.020 %0.020 %
 0.020 %0.020 %
Precipitation Temperature 70.0 - 90.0 °C158 - 194 °FCalibrator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10704 / 244171

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.