MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Freudenberg Sealing Technologies Ventoguard 471 Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

Information provided by Freudenberg Sealing Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc
@Temperature 23.0 °C
0.0408 lb/in³
@Temperature 73.4 °F
DIN EN ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70
@Temperature 23.0 °C
70
@Temperature 73.4 °F
DIN ISO 7619-1
Tensile Strength 15.0 MPa
@Temperature 23.0 °C
2180 psi
@Temperature 73.4 °F
DIN 53504, S2
Elongation at Break 287 %
@Temperature 23.0 °C
287 %
@Temperature 73.4 °F
DIN 53504, S2
100% Modulus 5.20 MPa
@Temperature 23.0 °C
754 psi
@Temperature 73.4 °F
DIN 53504, S2
Compression Set  28 %
@Temperature 70.0 °C,
Time 86400 sec
28 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815, B
 46 %
@Temperature 100 °C,
Time 86400 sec
46 %
@Temperature 212 °F,
Time 24.0 hour
DIN ISO 815, B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
Colorblack
Cross-linkingsulfur

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFREU9383 / 293902

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.