MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 899 X 120422 E Acetal (POM); Carbon Nanotube - Electrically Conductive
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccASTM D 792
Linear Mold Shrinkage 0.015 - 0.025 cm/cm
@Thickness 3.20 mm
0.015 - 0.025 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.7 MPa9100 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 2.07 GPa300 ksiASTM D 638
Flexural Strength 86.9 MPa12600 psiASTM D 790
Flexural Modulus 2.55 GPa370 ksiASTM D 790
Izod Impact, Notched 0.747 J/cm
@Thickness 3.20 mm
1.40 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 10.7 J/cm
@Thickness 3.20 mm
20.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 100 ohm-cm<= 100 ohm-cmASTM D 257
Surface Resistance 100 - 10000 ohm100 - 10000 ohmESD STM11.11
Surface Resistivity per Square 1000 ohm - 1e+051000 ohm - 1e+05ASTM D 257
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 218 °C360 - 425 °F
Mold Temperature 79.4 - 107 °C175 - 225 °F
Drying Temperature 121 °C
@Time 7200 sec
250 °F
@Time 2.00 hour
Moisture Content 0.15 %0.15 %
Dew Point -31.7 °C-25.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PQZUA13795 / 134664

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.