MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Ryton® R-4-02XT PPS, 40% glass fiber
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: 40% glass fiber, improved strength, black color

Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even at elevated temperatures.

Markets/Uses: Automotive / Automotive E/E / Connectors

Applications: Automotive Applications

Features: Chemical Resistant; Good Electrical Properties; Good Strength

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.69 g/cc0.0611 lb/in³ASTM D792
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.20 mm
0.0020 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 3.20 mm
0.0050 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 102102ASTM D785
Hardness, Rockwell R 120120ASTM D785
Tensile Strength 179 MPa26000 psiASTM D638
Tensile Stress 180 MPa26100 psiISO 527-2
Elongation at Break 1.4 %1.4 %ISO 527-2
 1.5 %1.5 %ASTM D638
Flexural Strength 255 MPa37000 psiASTM D790
 260 MPa37700 psiISO 178
Flexural Modulus 14.0 GPa2030 ksiISO 178
 14.5 GPa2100 ksiASTM D790
Compressive Strength 285 MPa41300 psiASTM D695
Poissons Ratio 0.390.39ASTM E132
Izod Impact, Notched 0.800 J/cm
@Thickness 3.18 mm
1.50 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.10 J/cm
@Thickness 3.18 mm
9.55 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²Notch A; ISO 180
Izod Impact, Unnotched (ISO) 30.0 kJ/m²14.3 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Insulation Resistance 1.00e+11 ohm
@Temperature 90.0 °C
1.00e+11 ohm
@Temperature 194 °F
IEC 60167
Dielectric Constant  3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
ASTM D150
 3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm559 kV/inASTM D149
Dissipation Factor  0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
ASTM D150
 0.0030
@Frequency 1e+6 Hz
0.0030
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 125 sec125 secASTM D495
Comparative Tracking Index 130 V130 VUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  15.0 µm/m-°C
@Temperature 100 - 200 °C
8.33 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
 20.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
11.1 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
CTE, linear, Transverse to Flow  40.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
22.2 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
 90.0 µm/m-°C
@Temperature 100 - 200 °C
50.0 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 200 - 220 °C392 - 428 °FUL Temperature Rating
Deflection Temperature at 1.8 MPa (264 psi) 265 °C509 °FUnannealed; ASTM D648
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 5VA
@Thickness 1.60 mm
5VA
@Thickness 0.0630 in
Oxygen Index 53 %53 %ASTM D2863
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4425 / 280225

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.