MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
PolyChem Alloy AquaGard™ 4504P
Categories: Polymer

Material Notes: AquaGard products are designed to improve the flame retardency of polyolefins without the use of halogen additives, such as bromine or chlorine. AquaGard products are available in a polyethylene or polypropylene carrier, and typically comply with UL94 fire and smoke regulations. Several grades are available, or Aguagard can be specifically formulated to satisfy individual requirements.

Processing Conditions: AquaGard 4504P can be blended into other resins (PE, PP) in a ratio of 7:3 (i.e 70 parts 4504P and 30 parts PE or PP). This ratio will impart flame retardancy, increase impact resistance and reduce elongation.

Information provided by the manufacturer, PolyChemAlloy.

Key Words: PolyChem Alloy, Zero halogen FR compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 - 1.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 38 - 42
Elongation at Yield 110 - 130 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 250 °C
 
Descriptive Properties
Active Content45 wt.%
CarrierPolyethylene
ColorOff-WhiteCustom colors available

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPC020 / 56049

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.